| Process
: |
|
1. Imported Prime logs e.g. Garjan and Keruing
constant moisturisation to prevent deterioration. |
 |
| |
|
| 2. Accurate peeling to produce face and core veneer. |
 |
| |
|
| 3. Telescopic Spindles and a back up roll mechanism. |
 |
| |
|
| 4. Stock and grading. |
 |
| |
|
| 5. Automatically controlled jet drying and dampening. |
 |
| |
|
6. Adhesive preparation
i. Phenol formaldehyde (PF) resins for marine plywood
ii. Non leachable organs - phoshp
preservatives for complete protection. |
 |
| |
|
7. Computer controlled hot pressing.
Thermic fluid wating system. |
 |
| |
|
8. Hot stacking for even celling
i. Reduces temperature gradients.
ii. Prevents warping.
iii. Aids post-press curing of the adhesive |
 |
| |
|
9. Pressure impregnating for powder proofing
i. Preservation acid-copper-chrome or
ACC treatment
ii. Pressure impregnation for a life time edge. |
 |
| |
|
10. Labelling of finished board Brand labels and
warranty statment ISI specifications and marks.
|
 |
| |
|